Promethium(III) oxide
Powdered promethium oxide in a metal tray
| |
Cubic form
| |
Hexagonal form
| |
Names | |
---|---|
IUPAC name
Promethium(III) oxide
| |
Other names
Promethium sesquioxide
| |
Identifiers | |
| |
3D model (JSmol)
|
|
PubChem CID
|
|
| |
| |
Properties | |
Pm2O3 | |
Molar mass | 337.824 g/mol |
Melting point | ~2320 °C[1] |
Structure | |
Cubic | |
Related compounds | |
Other anions
|
Promethium(III) chloride |
Other cations
|
Neodymium(III) oxide, Samarium(III) oxide, |
Except where otherwise noted, data are given for materials in their standard state (at 25 °C [77 °F], 100 kPa). | |
what is ?) | (|
Infobox references | |
Promethium(III) oxide is a compound with the formula Pm2O3. It is the most common form of promethium.
Crystal structure[]
Promethium oxide exists in three major crystalline forms:[1]
Form | Pearson symbol | Space group | No. | a,b,c (nm) | β(deg) | Z | Density (g/cm3) |
---|---|---|---|---|---|---|---|
Cubic | cI80 | Ia3 | 206 | 1.099 | 16 | 6.85 | |
Monoclinic | mS30 | C2/m | 12 | 1.422; 0.365; 0.891 | 100.1 | 6 | 7.48 |
Hexagonal | hP5 | P3m1 | 164 | 0.3802; 0.3802; 0.5954 | 1 | 7.62 |
*a, b and c are lattice parameters, Z is the number of formula units per unit cell, density is calculated from X-ray data.
The low-temperature cubic form converts to the monoclinic structure upon heating to 750–800 °C, and this transition can only be reversed by melting the oxide. The transition from the monoclinic to hexagonal form occurs at 1740 °C.
References[]
- ^ a b Chikalla, T. D.; McNeilly, C. E.; Roberts, F. P. (1972). "Polymorphic Modifications of Pm2O3". Journal of the American Ceramic Society. 55 (8): 428. doi:10.1111/j.1151-2916.1972.tb11329.x.